Thermoplastic comparison
PPS (polyphenylene sulfide) vs PVC, plasticized (flexible, PVC-P)
Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.
| Property | PPS (polyphenylene sulfide) | PVC, plasticized (flexible, PVC-P) | Difference |
|---|---|---|---|
| Density | 1.35 g/cm³ | 1.4 g/cm³ | PVC, plasticized (flexible, PVC-P) — 4% higher |
| Young's modulus E | 3.8 GPa | 1.4 GPa | PPS (polyphenylene sulfide) — 2.7× higher |
| Tensile strength | 80 MPa | 16 MPa | PPS (polyphenylene sulfide) — 5.0× higher |
| Glass transition Tg | 90 °C | 75 °C | PPS (polyphenylene sulfide) — 15 °C higher |
Where these numbers come from
- CAMPUS plastics database — typical grade datasheet values (campusplastics.com)
- MakeItFrom.com materials database — typical grade values
Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.