POM (acetal) vs PVC, plasticized (flexible, PVC-P)

Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

POM (acetal) in fullPVC, plasticized (flexible, PVC-P) in full← All materials
PropertyPOM (acetal)PVC, plasticized (flexible, PVC-P)Difference
Density1.41 g/cm³1.4 g/cm³POM (acetal) — 1% higher
Young's modulus E3.1 GPa1.4 GPaPOM (acetal) — 2.2× higher
Tensile strength65 MPa16 MPaPOM (acetal) — 4.1× higher
Glass transition Tg-60 °C75 °CPVC, plasticized (flexible, PVC-P) — 135 °C higher
  • CAMPUS plastics database — typical grade datasheet values (campusplastics.com)
  • MakeItFrom.com materials database — typical grade values

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.