Acrylic (PMMA) vs Polypropylene (PP)

Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

Acrylic (PMMA) in fullPolypropylene (PP) in full← All materials
PropertyAcrylic (PMMA)Polypropylene (PP)Difference
Density1.19 g/cm³0.905 g/cm³Acrylic (PMMA) — 31% higher
Young's modulus E3.1 GPa1.4 GPaAcrylic (PMMA) — 2.2× higher
Tensile strength72 MPa34 MPaAcrylic (PMMA) — 2.1× higher
Glass transition Tg105 °C-10 °CAcrylic (PMMA) — 115 °C higher
  • Callister & Rethwisch, Materials Science and Engineering, 10th ed.

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.