Thermoplastic comparison
PBT (polybutylene terephthalate) vs PVC, plasticized (flexible, PVC-P)
Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.
| Property | PBT (polybutylene terephthalate) | PVC, plasticized (flexible, PVC-P) | Difference |
|---|---|---|---|
| Density | 1.31 g/cm³ | 1.4 g/cm³ | PVC, plasticized (flexible, PVC-P) — 7% higher |
| Young's modulus E | 2.6 GPa | 1.4 GPa | PBT (polybutylene terephthalate) — 86% higher |
| Tensile strength | 55 MPa | 16 MPa | PBT (polybutylene terephthalate) — 3.4× higher |
| Glass transition Tg | 45 °C | 75 °C | PVC, plasticized (flexible, PVC-P) — 30 °C higher |
Where these numbers come from
- CAMPUS plastics database — typical grade datasheet values (campusplastics.com)
- MakeItFrom.com materials database — typical grade values
Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.