Polyamide 12 (PA12, Nylon 12) vs PVC, rigid (uPVC)

Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

Polyamide 12 (PA12, Nylon 12) in fullPVC, rigid (uPVC) in full← All materials
PropertyPolyamide 12 (PA12, Nylon 12)PVC, rigid (uPVC)Difference
Density1.01 g/cm³1.4 g/cm³PVC, rigid (uPVC) — 39% higher
Young's modulus E1.4 GPa3 GPaPVC, rigid (uPVC) — 2.1× higher
Tensile strength50 MPa48 MPaPolyamide 12 (PA12, Nylon 12) — 4% higher
Glass transition Tg45 °C82 °CPVC, rigid (uPVC) — 37 °C higher
  • CAMPUS plastics database — typical grade datasheet values (campusplastics.com)
  • Callister & Rethwisch, Materials Science and Engineering, 10th ed.

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.