Thermoplastic comparison
ABS vs Polypropylene (PP)
Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.
| Property | ABS | Polypropylene (PP) | Difference |
|---|---|---|---|
| Density | 1.05 g/cm³ | 0.905 g/cm³ | ABS — 16% higher |
| Young's modulus E | 2.3 GPa | 1.4 GPa | ABS — 64% higher |
| Tensile strength | 44 MPa | 34 MPa | ABS — 29% higher |
| Glass transition Tg | 105 °C | -10 °C | ABS — 115 °C higher |
Where these numbers come from
- CAMPUS plastics database — typical grade datasheet values (campusplastics.com)
- Callister & Rethwisch, Materials Science and Engineering, 10th ed.
Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.