Polystyrene (GPPS) vs UHMW-PE (ultra-high-molecular-weight polyethylene)

Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

Polystyrene (GPPS) in fullUHMW-PE (ultra-high-molecular-weight polyethylene) in full← All materials
PropertyPolystyrene (GPPS)UHMW-PE (ultra-high-molecular-weight polyethylene)Difference
Density1.05 g/cm³0.94 g/cm³Polystyrene (GPPS) — 12% higher
Young's modulus E3.2 GPa0.8 GPaPolystyrene (GPPS) — 4.0× higher
Tensile strength46 MPa49 MPaUHMW-PE (ultra-high-molecular-weight polyethylene) — 7% higher
Glass transition Tg100 °C-120 °CPolystyrene (GPPS) — 220 °C higher
  • Callister & Rethwisch, Materials Science and Engineering, 10th ed.
  • MakeItFrom.com materials database — typical grade values

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.