POM (acetal) vs Polysulfone (PSU)

Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

POM (acetal) in fullPolysulfone (PSU) in full← All materials
PropertyPOM (acetal)Polysulfone (PSU)Difference
Density1.41 g/cm³1.24 g/cm³POM (acetal) — 14% higher
Young's modulus E3.1 GPa2.5 GPaPOM (acetal) — 24% higher
Tensile strength65 MPa70 MPaPolysulfone (PSU) — 8% higher
Glass transition Tg-60 °C185 °CPolysulfone (PSU) — 245 °C higher
  • CAMPUS plastics database — typical grade datasheet values (campusplastics.com)

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.