Thermoplastic comparison
POM (acetal) vs Polystyrene (GPPS)
Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.
| Property | POM (acetal) | Polystyrene (GPPS) | Difference |
|---|---|---|---|
| Density | 1.41 g/cm³ | 1.05 g/cm³ | POM (acetal) — 34% higher |
| Young's modulus E | 3.1 GPa | 3.2 GPa | Polystyrene (GPPS) — 3% higher |
| Tensile strength | 65 MPa | 46 MPa | POM (acetal) — 41% higher |
| Glass transition Tg | -60 °C | 100 °C | Polystyrene (GPPS) — 160 °C higher |
Where these numbers come from
- CAMPUS plastics database — typical grade datasheet values (campusplastics.com)
- Callister & Rethwisch, Materials Science and Engineering, 10th ed.
Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.