Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

PET in fullUHMW-PE (ultra-high-molecular-weight polyethylene) in full← All materials
PropertyPETUHMW-PE (ultra-high-molecular-weight polyethylene)Difference
Density1.37 g/cm³0.94 g/cm³PET — 46% higher
Young's modulus E2.9 GPa0.8 GPaPET — 3.6× higher
Tensile strength60 MPa49 MPaPET — 22% higher
Glass transition Tg76 °C-120 °CPET — 196 °C higher
Melting point Tm255 °C130 °CPET — 125 °C higher
  • Callister & Rethwisch, Materials Science and Engineering, 10th ed.
  • MakeItFrom.com materials database — typical grade values

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.