| Property | PEI (Ultem) | Acrylic (PMMA) | Difference |
|---|---|---|---|
| Density | 1.27 g/cm³ | 1.19 g/cm³ | PEI (Ultem) — 7% higher |
| Young's modulus E | 3.2 GPa | 3.1 GPa | PEI (Ultem) — 3% higher |
| Tensile strength | 105 MPa | 72 MPa | PEI (Ultem) — 46% higher |
| Glass transition Tg | 217 °C | 105 °C | PEI (Ultem) — 112 °C higher |
Where these numbers come from
- CAMPUS plastics database — typical grade datasheet values (campusplastics.com)
- Callister & Rethwisch, Materials Science and Engineering, 10th ed.
Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.