Polyamide 6 (PA6, Nylon 6) vs PET

Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

Polyamide 6 (PA6, Nylon 6) in fullPET in full← All materials
PropertyPolyamide 6 (PA6, Nylon 6)PETDifference
Density1.13 g/cm³1.37 g/cm³PET — 21% higher
Young's modulus E2.8 GPa2.9 GPaPET — 4% higher
Tensile strength78 MPa60 MPaPolyamide 6 (PA6, Nylon 6) — 30% higher
Glass transition Tg50 °C76 °CPET — 26 °C higher
Melting point Tm220 °C255 °CPET — 35 °C higher
  • Callister & Rethwisch, Materials Science and Engineering, 10th ed.

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.