Polyamide 12 (PA12, Nylon 12) vs Polystyrene (GPPS)

Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

Polyamide 12 (PA12, Nylon 12) in fullPolystyrene (GPPS) in full← All materials
PropertyPolyamide 12 (PA12, Nylon 12)Polystyrene (GPPS)Difference
Density1.01 g/cm³1.05 g/cm³Polystyrene (GPPS) — 4% higher
Young's modulus E1.4 GPa3.2 GPaPolystyrene (GPPS) — 2.3× higher
Tensile strength50 MPa46 MPaPolyamide 12 (PA12, Nylon 12) — 9% higher
Glass transition Tg45 °C100 °CPolystyrene (GPPS) — 55 °C higher
  • CAMPUS plastics database — typical grade datasheet values (campusplastics.com)
  • Callister & Rethwisch, Materials Science and Engineering, 10th ed.

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.