Polyamide 12 (PA12, Nylon 12) vs PET

Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

Polyamide 12 (PA12, Nylon 12) in fullPET in full← All materials
PropertyPolyamide 12 (PA12, Nylon 12)PETDifference
Density1.01 g/cm³1.37 g/cm³PET — 36% higher
Young's modulus E1.4 GPa2.9 GPaPET — 2.1× higher
Tensile strength50 MPa60 MPaPET — 20% higher
Glass transition Tg45 °C76 °CPET — 31 °C higher
Melting point Tm178 °C255 °CPET — 77 °C higher
  • CAMPUS plastics database — typical grade datasheet values (campusplastics.com)
  • Callister & Rethwisch, Materials Science and Engineering, 10th ed.

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.