Polyethylene, high-density (HDPE) vs POM (acetal)

Every value below is a typical room-temperature figure with its source, test method and conditions — the same dataset that drives the calculators.

Polyethylene, high-density (HDPE) in fullPOM (acetal) in full← All materials
PropertyPolyethylene, high-density (HDPE)POM (acetal)Difference
Density0.95 g/cm³1.41 g/cm³POM (acetal) — 48% higher
Young's modulus E1 GPa3.1 GPaPOM (acetal) — 3.1× higher
Tensile strength27 MPa65 MPaPOM (acetal) — 2.4× higher
Glass transition Tg-120 °C-60 °CPOM (acetal) — 60 °C higher
Melting point Tm131 °C175 °CPOM (acetal) — 44 °C higher
  • Callister & Rethwisch, Materials Science and Engineering, 10th ed.
  • CAMPUS plastics database — typical grade datasheet values (campusplastics.com)

Typical room-temperature values for learning and preliminary design; grades vary widely and a supplier datasheet always overrides a textbook figure. Confirm against the datasheet before design work.